MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beryllium-Copper Alloy 50C, UNS C81800, Cast and Aged
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, Permanent Mold, Plaster, and Sand.

Applications: Resistance welding electrodes, dies

Test specimen: cast and aged 3 hours at 480°C.

Inactive per the Copper Development Association.

Key Words: BeCu; beryllium copper alloy 50C, CA 818, RWMA Class III
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.62 g/cc0.311 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7070
Tensile Strength, Ultimate 450 MPa65300 psi
Tensile Strength, Yield 275 MPa
@Strain 0.2 %
39900 psi
@Strain 0.2 %
Elongation at Break 15 %15 %In 50 mm
Modulus of Elasticity 110 GPa16000 ksi
Poissons Ratio 0.330.33
Shear Modulus 41.0 GPa5950 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000359 ohm-cm
@Temperature 20.0 °C
0.0000359 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 218 W/m-K
@Temperature 20.0 °C
1510 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1010 - 1070 °C1850 - 1960 °F
Solidus 1010 °C1850 °F
Liquidus 1070 °C1960 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Solution Temperature 900 - 925 °C1650 - 1700 °F
Aging Temperature 480 °C896 °F
Casting Temperature 1120 - 1175 °C2050 - 2147 °FHeavy castings
 1175 - 1230 °C2147 - 2250 °FLight castings
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.10 %<= 0.10 %
Beryllium, Be 0.30 - 0.55 %0.30 - 0.55 %
Chromium, Cr <= 0.10 %<= 0.10 %
Cobalt, Co 1.4 - 1.7 %1.4 - 1.7 %
Copper, Cu >= 95.6 %>= 95.6 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.0020 %<= 0.0020 %
Nickel, Ni <= 0.20 %<= 0.20 %
Silicon, Si <= 0.15 %<= 0.15 %
Silver, Ag 0.080 - 0.12 %0.080 - 0.12 %
Tin, Sn <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium-Copper Alloy 50C, UNS C81800, As-cast
Beryllium Copper Alloy 10C, UNS C82000 Cast and Aged
Beryllium Copper 21C UNS C82510 Casting Alloy Cast and Aged
Beryllium-Copper Alloy 30C, UNS C82200, Cast and Aged
UNS C81400, Copper Casting Alloy

MC81800b3 / 11863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.