MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Filler Content 8.0 %8.0 %Carbon Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 86.2 MPa12500 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 5.0 - 10 %5.0 - 10 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.07 GPa300 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 172 MPa24900 psiASTM D790
Flexural Modulus 2.76 GPa400 ksiASTM D790
Izod Impact, Notched 0.910 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.70 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 5.00e+8 - 5.00e+12 ohm5.00e+8 - 5.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 139 °C
@Thickness 6.35 mm
282 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 133 °C
@Thickness 6.35 mm
271 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Flammability, UL94  V-0
@Thickness 0.794 mm
V-0
@Thickness 0.0313 in
Internal Method
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Internal Method
 V-0
@Thickness 3.15 mm
V-0
@Thickness 0.124 in
Internal Method
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 290 - 310 °C554 - 590 °F
Middle Barrel Temperature 290 - 310 °C554 - 590 °F
Front Barrel Temperature 290 - 310 °C554 - 590 °F
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
 
Descriptive Properties
AdditiveAntistatic
FeaturesAntistatic
 Electromagnetic Shielding (EMI)
 ESD Protection
 Flame Retardant
 Radio Frequency Shielding (RFI)
FormsPellets
Generic MaterialPC
Generic NamePolycarbonate (PC)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAerospace Applications
 Automotive Under the Hood
 Business Equipment
 Electrical/Electronic Applications
 Housings
 Printer Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOY GP1000LG PC, Transparent
Avient Trilliant™ HC HC3220-0030 RS Natural Polycarbonate (PC)
Mitsubishi Iupilon® FPR 3500 Polycarbonate
Clariant Renol PCSP0015 Polycarbonate, Carbon Fiber Filled
Clariant Renol PCSP0009 Polycarbonate, 15% Glass Fiber, Silicone Lubricated

PH0POL0680 / 145249

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.