MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cadi MOLD-MOR™ 2
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical and thermal electrical conductivity are required.

Forms:

  • Rod
  • Bar
  • Plate

Information provided by Cadi Company.

Key Words: ASTM B441, ASTM B534, UNS C17510
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.77 g/cc0.317 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B >= 90>= 90Any thickness
Tensile Strength at Break  >= 607 MPa
@Thickness >=50.8 mm
>= 88000 psi
@Thickness >=2.00 in
 >= 621 MPa
@Thickness 25.4 - 50.8 mm
>= 90000 psi
@Thickness 1.00 - 2.00 in
 >= 648 MPa
@Thickness <=25.4 mm
>= 94000 psi
@Thickness <=1.00 in
Tensile Strength, Yield  >= 607 MPa
@Strain 0.5 %,
Thickness >=50.8 mm
>= 88000 psi
@Strain 0.5 %,
Thickness >=2.00 in
 >= 621 MPa
@Strain 0.5 %,
Thickness 25.4 - 50.8 mm
>= 90000 psi
@Strain 0.5 %,
Thickness 1.00 - 2.00 in
 >= 648 MPa
@Strain 0.5 %,
Thickness <=25.4 mm
>= 94000 psi
@Strain 0.5 %,
Thickness <=1.00 in
Modulus of Elasticity 131 GPa19000 ksi
Poissons Ratio 0.2670.267
Shear Modulus 51.7 GPa7500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00000383 ohm-cm<= 0.00000383 ohm-cm>45% IACS, up to 3" diameter/any thickness
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 225 W/m-K1560 BTU-in/hr-ft²-°F
Melting Point 1029 - 1068 °C1885 - 1955 °F
Solidus 1029 °C1885 °F
Liquidus 1068 °C1955 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 788 °C1450 °FBrazing
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.40 %0.40 %
Copper, Cu 97.8 %97.8 %
Nickel, Ni 1.8 %1.8 %
 
Descriptive Properties
RMWA Class3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® 100 Copper Alloy
Architectural Bronze, UNS C38500
Brush Wellman Beryllium Copper Alloy 3 Strip; A-Dead Soft (TB00) Temper (UNS C17510)
Cadi MOLD-MOR™ 20
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; A (TB00) Temper (UNS C17510)

NCADI05 / 15513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.