MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Stress Relieved
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal; Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new material has corrosion resistance superior to that of Type 430FR Solenoid Quality stainless with generally similar magnetic properties. It is stabilized by niobium (columbium) to provide improved corrosion resistance with optimum machinability. The alloy balance also provides resistivity similar to that of Type 430FR Solenoid Quality stainless. High resistivity is beneficial in applications involving AC excitation due to the suppression of eddy current losses.

Chrome Core® is a registered trademark of Carpenter Technology Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8686
Tensile Strength, Ultimate 517 MPa75000 psi
Tensile Strength, Yield 345 MPa
@Strain 0.2 %
50000 psi
@Strain 0.2 %
Elongation at Break 35 %35 %In 4D
Reduction of Area 64 %64 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.4 µm/m-°C
@Temperature 23.0 - 204 °C
5.78 µin/in-°F
@Temperature 73.4 - 399 °F
 11.5 µm/m-°C
@Temperature 23.0 - 427 °C
6.39 µin/in-°F
@Temperature 73.4 - 801 °F
 13.1 µm/m-°C
@Temperature 23.0 - 982 °C
7.28 µin/in-°F
@Temperature 73.4 - 1800 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.015 %0.015 %
Chromium, Cr 17.5 %17.5 %
Iron, Fe 79 %79 %as remainder
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 1.75 %1.75 %
Nickel, Ni 0.20 %0.20 %
Niobium, Nb (Columbium, Cb) 0.25 %0.25 %
Phosphorus, P 0.020 %0.020 %
Silicon, Si 0.90 %0.90 %
Sulfur, S 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Annealed
AISI Type 430F Stainless Steel
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel
Schmolz + Bickenbach 430FR Stainless Steel Bar

NCARG5 / 15766

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.