System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Ineos ABS NOVODUR® P3TF ABS, Injection Grade
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
Injection molding grade, improved flow.
Applications:
Automotive industry: e.g. wheel trims, instrument panel components.
Novodur® is now a product of INEOS Styrolution. Information provided by the manufacturer.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.06
g/cc
0.0383
lb/in³
Water Absorption at Saturation
0.30 %
0.30 %
0.30 %
0.30 %
Melt Flow
4.0
g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.0
g/10 min
@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
55.0
MPa
7980
psi
Elongation at Yield
2.6 %
2.6 %
Tensile Modulus
3.00
GPa
435
ksi
Electrical Properties
Metric
English
Comments
Electrical Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
Surface Resistance
1.00e+15
ohm
1.00e+15
ohm
Dielectric Constant
2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Dielectric Strength
31.0
kV/mm
787
kV/in
Dissipation Factor
0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
Comparative Tracking Index
600
V
600
V
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
80.0
µm/m-°C
@Temperature 20.0 °C
44.4
µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi)
108
°C
226
°F
Deflection Temperature at 1.8 MPa (264 psi)
101
°C
214
°F
Vicat Softening Point
112
°C
234
°F
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Ineos ABS NOVODUR® P2L-AT ABS, Injection Grade
Ineos ABS LUSTROPAK® 1020 ABS, Extrusion Grade
Ineos ABS Lustran® QE 1088 FC, Injection Grade
Hannam Chemical Hanalac 775 ABS, Extrusion Grade
Hannam Chemical Hanalac 770 ABS, Extrusion Grade
PBA511 / 26983
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.