MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

3D Systems LaserForm® Maraging Steel (B), AS BUILT
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Tool Steel

Material Notes: Maraging Steel fine-tuned for use with ProX® DMP 200 and ProX® DMP 300 metal printers producing industrial parts and tool inserts with a combination of high-strength and excellent hardness. LaserForm Maraging Steel (B) is formulated and fine-tuned specifically for 3D Systems ProX DMP 200 and 300 metal 3D printers to deliver high part quality and consistent part properties.

With properties like 1.2709, this steel is easily heat-treatable in a simple age-hardening process resulting in excellent hardness and strength. LaserForm Maraging Steel (B) has good wear resistance. In regards to post-processing, the material shows good weldability and machinability. LaserForm Maraging Steel (B) is ideal for innovative tool and mold designs including conformal cooling channels for injection molding, die casting and extrusion. The material is also used for high-performance aerospace, automotive and other industrial applications which require high strength and wear resistance.

Classification: The chemical composition of LaserForm Maraging Steel (B) with additional restrictions compared to the DIN 1.2709 standards.

Information provided by 3D Systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.06 g/cc0.291 lb/in³Absolute theoretical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 34 - 3834 - 38ASTM E18
Tensile Strength, Ultimate 1010 - 1090 MPa146000 - 158000 psiVertical direction - Z; ASTM E8M
 1160 - 1200 MPa168000 - 174000 psiHorizontal direction - XY; ASTM E8M
Tensile Strength, Yield 720 - 840 MPa104000 - 122000 psiRp0.2%, Vertical direction - Z; ASTM E8M
 890 - 1010 MPa129000 - 146000 psiRp0.2%, Horizontal direction - XY; ASTM E8M
Elongation at Break 10 - 16 %10 - 16 %Horizontal direction - XY; ASTM E8M
 10 - 16 %10 - 16 %Vertical direction - Z; ASTM E8M
Reduction of Area 50 - 60 %50 - 60 %Horizontal direction - XY; ASTM E8M
 55 - 65 %55 - 65 %Vertical direction - Z; ASTM E8M
Tensile Modulus 11.5 - 17.5 GPa1670 - 2540 ksiYoungs, Vertical direction - Z; ASTM E8M
 13.0 - 19.0 GPa1890 - 2760 ksiYoungs, Horizontal direction — XY; ASTM E8M
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000440 ohm-cm0.0000440 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C
@Temperature 20.0 - 600 °C
5.56 µin/in-°F
@Temperature 68.0 - 1110 °F
Thermal Conductivity 20.9 W/m-K145 BTU-in/hr-ft²-°F
Melting Point 1430 - 1450 °C2610 - 2640 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Cobalt, Co 9.0 - 11 %9.0 - 11 %
Iron, Fe 60.87 - 69.1 %60.87 - 69.1 %Balance
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 4.0 - 6.0 %4.0 - 6.0 %
Nickel, Ni 17 - 19 %17 - 19 %
Silicon, Si <= 1.0 %<= 1.0 %
Titanium, Ti 0.90 - 1.1 %0.90 - 1.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type H13 Hot Work Tool Steel
Aperam AFK 18 Cold Rolled Strip
ATI Allegheny Ludlum H13 Tool Steel, UNS T20813
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48
Latrobe MP35N® Alloy

PAPPR3128 / 239096

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.