MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram RamTal PM7013 Acetal, UV Stabilized
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Polyacetal copolymer UV stabilized for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³DIN 53479
Water Absorption 0.22 %0.22 %DIN 53495
Linear Mold Shrinkage 0.018 - 0.022 cm/cm0.018 - 0.022 in/in
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8282ASTM-D785
Tensile Strength, Yield 65.0 MPa9430 psiASTM-D638
Elongation at Break 25 %25 %ASTM-D638
Flexural Strength 85.0 MPa12300 psiASTM-D790
Flexural Modulus 2.80 GPa406 ksiASTM-D790
Izod Impact, Notched 0.600 J/cm
@Temperature 23.0 °C
1.12 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmDIN 53482
Surface Resistance 1.00e+14 ohm1.00e+14 ohmDIN 53482
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 24.0 kV/mm610 kV/inVDE 0303/4
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FDIN 53461

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® GVX-7 H nat PA*-GF70
Eastman Tritan™ MXF121 Medical Grade Copolyester
Delrin Delrin® 100 NC010 POM
Polyram RamTal RM7009 Acetal, UV Stabilized
Polyram RamTal PM7109 Acetal, UV Stabilized

PPOLYRA117 / 57379

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.