MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sweet Birch Wood
Categories: Wood and Natural Products; Wood; Hardwood

Key Words: Betula Lenta; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.600 g/cc0.600 g/ccGreen, based on volume
 0.650 g/cc0.650 g/cc12% moisture content, based on volume
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 4315 N970.1 lb (f)Green
 6539 N1470 lb (f)12% moisture content
Tensile Strength at Break 2.96 MPa430 psiGreen, perpendicular to grain
 6.55 MPa950 psi12% moisture content, perpendicular to grain
Modulus of Elasticity 11.4 GPa1650 ksiGreen
 15.0 GPa2170 ksi12% moisture content
Modulus of Rupture 0.0648 GPa9.40 ksiGreen
 0.117 GPa16.9 ksi12% moisture content
Compressive Strength 3.24 MPa470 psiGreen, perpendicular to grain
 7.45 MPa1080 psi12% moisture content, perpendicular to grain
 25.8 MPa3740 psiGreen, parallel to grain
 58.9 MPa8540 psi12% moisture content, parallel to grain
Shear Strength 8.55 MPa1240 psiGreen, parallel to grain
 15.4 MPa2240 psi12% moisture content, parallel to grain
Impact 4747Impact bending in inches, 12% moisture content
 4848Impact bending in inches, green
Work to Maximum Load 0.108 J/cm³15.7 in-lb/in³Green
 0.124 J/cm³18.0 in-lb/in³12% moisture content
 
Thermal PropertiesMetricEnglishComments
Shrinkage 6.5 %6.5 %Radial, from green to oven dry, US origin
 9.0 %9.0 %Tangential, from green to oven dry, US origin
 15.6 %15.6 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Yellow Birch Wood
Paper Birch Wood
Black Maple Wood
Bigleaf Maple Wood
American Maple, Rock (Sugar Maple)

PTSU017 / 71459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.