MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical properties and enhanced sealability. It contains antioxidant additives. Its applications include: stretch films; liners; LDPE and HDPE blends and packages for general use; blends for irrigation pipes; and insulation for low and medium tension XLPE wires and cables. Recommended processing conditions for film extrusion are about 170 - 210 ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM-D1505
Melt Flow 2.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 1220 %1220 %ASTM-D882
Film Elongation at Break, TD 1440 %1440 %ASTM-D882
Elmendorf Tear Strength MD 120 g120 gASTM-D1922
Elmendorf Tear Strength TD 340 g340 gASTM-D1922
Elmendorf Tear Strength, MD 3.16 g/micron80.3 g/milASTM-D1922
Elmendorf Tear Strength, TD 8.95 g/micron227 g/milASTM-D1922
Dart Drop 2.37 g/micron60.2 g/milASTM-D1709
Dart Drop Test 90.0 g0.198 lbASTM-D1709
Film Tensile Strength at Break, MD 30.0 MPa4350 psiASTM-D882
Film Tensile Strength at Break, TD 30.0 MPa4350 psiASTM-D882
1% Secant Modulus, MD 180 MPa26100 psiASTM-D882
1% Secant Modulus, TD 200 MPa29000 psiASTM-D882
 
Optical PropertiesMetricEnglishComments
Haze 61 %61 %ASTM-D1003
Gloss 19 %19 %Angle 60°; ASTM-D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene
Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer
Chevron Phillips Marlex® 9607 HDPE Cast Film Resin
Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene

PBRAS870 / 106716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.