MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bisalloy Steels BisPlate 80PV Thickness 6-<16 mm
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel; Pressure Vessel Steel

Material Notes: A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.

Applications: Transport Road Tankers, Storage Tanks, Railroad Tankers, Refinery and Petro Chemical Equipment

Testing: AS/NZS 3597 Grade 700PV NATA approved

Welding: According to AS/NZS 1554 parts 4 and 5

Tolerance: In accordance with AS/NZS 1365

Key Words: ASTM A517, EN 10028-6 Grade P690Q
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 255255
Tensile Strength at Break 830 MPa120000 psi
Tensile Strength, Yield 750 MPa
@Strain 0.2 %
109000 psi
@Strain 0.2 %
Elongation at Break 26 %26 %in 50 mm GL
Charpy Impact 55.0 J
@Temperature -20.0 °C
40.6 ft-lb
@Temperature -4.00 °F
Transverse
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.0010 %0.0010 %
Carbon, C 0.16 %0.16 %
Iron, Fe 98.3 %98.3 %As Balance
Manganese, Mn 1.1 %1.1 %
Molybdenum, Mo 0.20 %0.20 %
Phosphorus, P 0.010 %0.010 %
Silicon, Si 0.20 %0.20 %
Sulfur, S 0.0030 %0.0030 %
 
Descriptive Properties
CE (IIW)0.4
PCM0.25
Surface FinishShotblasted

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A285, Grade A
Bisalloy Steels BisPlate 80PV Thickness 16-80 mm
ASTM A285, Grade C
Outokumpu 904L High Performance Austenitic Stainless Steel
ASTM A414 Grade A Pressure Vessel Steel, Composition Spec

NBISAL18 / 15465

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.