MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BNZ Materials Blazecrete 2800 Dense Castable
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory furnace upper side walls and roofs.

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.05 g/cc0.0741 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00620 GPa0.899 ksiAt Use Limit; ASTM C268
 0.00100 GPa
@Temperature 815 °C
0.145 ksi
@Temperature 1500 °F
ASTM C268
 0.00140 GPa
@Temperature 540 °C
0.203 ksi
@Temperature 1000 °F
Fired; ASTM C268
 0.00140 GPa
@Temperature 1095 °C
0.203 ksi
@Temperature 2003 °F
ASTM C268
 0.00210 GPa
@Temperature 1260 °C
0.305 ksi
@Temperature 2300 °F
ASTM C268
 0.00340 GPa
@Temperature 104 °C
0.493 ksi
@Temperature 219 °F
Dried; ASTM C268
 0.00340 GPa
@Temperature 1371 °C
0.493 ksi
@Temperature 2500 °F
ASTM C268
Compressive Strength  9.00 MPa
@Temperature 1095 °C
1310 psi
@Temperature 2003 °F
Cold Crush Strength
 15.2 MPa
@Temperature 1260 °C
2200 psi
@Temperature 2300 °F
Cold Crush Strength
 17.2 MPa
@Temperature 815 °C
2490 psi
@Temperature 1500 °F
Cold Crush Strength
 35.1 MPa
@Temperature 1371 °C
5090 psi
@Temperature 2500 °F
Cold Crush Strength
 48.8 MPa
@Temperature 1556 °C
7080 psi
@Temperature 2833 °F
Cold Crush Strength; At Use Limit
 15.2 MPa
@Treatment Temp. 540 °C
2200 psi
@Treatment Temp. 1000 °F
Cold Crush Strength; Dried 104°C
 20.7 MPa
@Treatment Temp. 104 °C
3000 psi
@Treatment Temp. 219 °F
Cold Crush Strength; Dried 104°C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1537 °C2799 °F
Shrinkage  0.00 %
@Temperature 104 °C
0.00 %
@Temperature 219 °F
Permanent Linear Change; ASTM C210
 0.00 %
@Temperature 1260 °C
0.00 %
@Temperature 2300 °F
Permanent Linear Change; ASTM C210
 0.10 %
@Temperature 540 °C
0.10 %
@Temperature 1000 °F
Permanent Linear Change; ASTM C210
 0.10 %
@Temperature 815 °C
0.10 %
@Temperature 1500 °F
Permanent Linear Change; ASTM C210
 0.20 %
@Temperature 1095 °C
0.20 %
@Temperature 2003 °F
Permanent Linear Change; ASTM C210
 1.0 %
@Temperature 1556 °C
1.0 %
@Temperature 2833 °F
Permanent Linear Change at Use Limit
 
Component Elements PropertiesMetricEnglishComments
Al2O3 45.5 %45.5 %
CaO 5.6 %5.6 %
Fe2O3 3.4 %3.4 %
MgO 0.10 %0.10 %
Na2O 0.30 %0.30 %Includes K2O
SiO2 43.1 %43.1 %
TiO2 1.9 %1.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ametek High Purity Nickel Strip 899A Annealed
Gray Cast Iron, ASTM A 48 Class 40
Cobalt, Co
Copper, Cu; Annealed
Overview of materials for Nylon 6, Cast

CBNZ952 / 149192

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.