MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® KR 4350 PA6/6T (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain constant after moisture absorption up to a temperature of 60°C [140°F].

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.6 - 2.0 %1.6 - 2.0 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 6.5 - 7.5 %6.5 - 7.5 %ISO 62
Viscosity Measurement 130130ISO 307
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inrestricted
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  10.0 MPa
@Strain 2 %,
Temperature 100 °C
1450 psi
@Strain 2 %,
Temperature 212 °F
50mm/min
 40.0 MPa
@Strain 2 %,
Temperature 80.0 °C
5800 psi
@Strain 2 %,
Temperature 176 °F
50mm/min
 60.0 MPa
@Strain 2 %,
Temperature 60.0 °C
8700 psi
@Strain 2 %,
Temperature 140 °F
50mm/min
 75.0 MPa
@Strain 2 %,
Temperature 23.0 °C
10900 psi
@Strain 2 %,
Temperature 73.4 °F
50mm/min
Tensile Strength, Yield 100 MPa14500 psi50 mm/min; ISO 527-1/-2
Tensile Stress at Strain  20.0 MPa
@Strain 5.0 %,
Temperature 100 °C
2900 psi
@Strain 5.0 %,
Temperature 212 °F
50mm/min
 25.0 MPa
@Strain 8.0 %,
Temperature 100 °C
3630 psi
@Strain 8.0 %,
Temperature 212 °F
50mm/min
 50.0 MPa
@Strain 5.0 %,
Temperature 80.0 °C
7250 psi
@Strain 5.0 %,
Temperature 176 °F
50mm/min
 50.0 MPa
@Strain 8.0 %,
Temperature 80.0 °C
7250 psi
@Strain 8.0 %,
Temperature 176 °F
50mm/min
 73.0 MPa
@Strain 8.0 %,
Temperature 60.0 °C
10600 psi
@Strain 8.0 %,
Temperature 140 °F
50mm/min
 75.0 MPa
@Strain 5.0 %,
Temperature 60.0 °C
10900 psi
@Strain 5.0 %,
Temperature 140 °F
50mm/min
 80.0 MPa
@Strain 8.0 %,
Temperature 23.0 °C
11600 psi
@Strain 8.0 %,
Temperature 73.4 °F
50mm/min
 110 MPa
@Strain 5.0 %,
Temperature 23.0 °C
16000 psi
@Strain 5.0 %,
Temperature 73.4 °F
50mm/min
Elongation at Yield 8.0 %8.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 3.20 GPa464 ksiISO 527-1/-2
 1.75 GPa
@Temperature 100 °C
254 ksi
@Temperature 212 °F
ISO 527
 3.00 GPa
@Temperature 80.0 °C
435 ksi
@Temperature 176 °F
ISO 527
 3.50 GPa
@Temperature 60.0 °C
508 ksi
@Temperature 140 °F
ISO 527
 3.75 GPa
@Temperature 40.0 °C
544 ksi
@Temperature 104 °F
ISO 527
Flexural Modulus 2.90 GPa421 ksiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched  10.5 J/cm²
@Temperature -30.0 °C
50.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 - 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
33.3 - 44.4 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FDIN 52612
Melting Point 295 °C563 °FDIN 53765
Maximum Service Temperature, Air 110 °C230 °Ffor 50% loss of tensile strength after 20000hr
 130 °C266 °Ffor 50% loss of tensile strength after 5000hr
 250 °C482 °F
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 330 °C590 - 626 °FInjection-molding/Extrusion
Mold Temperature 70.0 - 100 °C158 - 212 °FInjection-molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 40 1 L black (4581) PA6 + PP Dry, 40% Glass Filled, Heat Stabilized
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry)
Asahi Kasei Leona™ 14G25 Polyamide 66, Heat Stabilized, GF Reinforced
BASF Ultramid® 8202 PA6 (Conditioned)

PBASG0282 / 131915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.