MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Thermal Ceramics Cerafiber® Bulk Fiber
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Cerafiber, a high-purity synthetic blend of alumina and silica, is manufactured using the melt spinning process as are all “Cera” fibers.

Engineered Fibers - Kaowool Engineered fibers are based on our extensive family of bulks. Value adding technology has been developed to allow Thermal Ceramics to tailor products to meet specific customer requirements. Fiber length, diameter, and surface treatment can be engineered as can the fiber content. Thermal Ceramics can work with you to produce a Kaowool Engineered Fiber to meet unique requirements. The various grades of fibers can be engineered for applications in plastic reinforcement, metal matrix composites, and automotive applications. Kaowool Bulk Fiber can be used as high-temperature loose fill or packing material in a variety of applications including expansion joint construction, furnace walls and base seals, low mass kiln car top construction, tube seal fabrication, and packing around hard refractory furnace components such as burner blocks.

These products are also used in secondary processes such as felting, vacuum forming boards and shapes, and the manufacture of specialty papers, textiles, high-temperature adhesives and moldable products.

Thermal Ceramics bulk fibers offer a maximum temperature range of between 2300° and 3000°F (1260° to 1549°C). They also provide excellent chemical stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acids, and strong alkalis. If wet by oil or water, thermal and physical properties will be fully restored after drying.

Compared to other refractory materials, bulk fibers and products made from them are lightweight, resistant to thermal shock, and provide a low thermal conductivity. The sound absorption capabilities of Thermal Ceramics bulk fibers are far superior than those of dense refractories or other insulating refractories.

Information provided by Thermal Ceramics

Data has not been recently verified. Please contact manufacturer for current information.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.65 g/cc2.65 g/ccASTM C135
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.089 J/g-°C
@Temperature 982 °C
0.2602 BTU/lb-°F
@Temperature 1800 °F
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1180 °C2150 °FContinuous
 1320 °C2400 °FRating
 
Component Elements PropertiesMetricEnglishComments
Al2O3 46 %46 %
SiO2 54 %54 %
 
Descriptive Properties
Other Element Contenttraces

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SPHERE ONE EXTENDOSPHERES™ MG Hollow Spheres
SPHERE ONE EXTENDOSPHERES™ FM-1 Hollow Spheres
SPHERE ONE EXTENDOSPHERES™ 350 Hollow Spheres
Novum Glass Solid Soda-lime Uniform Series Glass Microspheres
Imerys NYGLOS® 12 Wollastonite

CTHERM027 / 2347

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.