MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® LB Polyester Film, 92 Gauge (23 µm)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Varieties with enhanced surface characteristics for bonding by inks, primers, and adhesives. A basic lamination would combine plain or printed LB with a heat sealable ply consisting of LDPE, LLDPE, EVA, ionomer, acid copolymer, PVC, or other materials using adhesive or extrusion laminating techniques.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Average value for Mylar® films.
Moisture Vapor Transmission 0.500 cc-mm/m²-24hr-atm1.27 cc-mil/100 in²-24hr-atmASTM E96 Procedure E
Water Vapor Transmission 20.0 g/m²/day1.29 g/100 in²/dayASTM E96 Procedure E
Oxygen Transmission 1.70 cc-mm/m²-24hr-atm4.32 cc-mil/100 in²-24hr-atmor 75 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 23.0 microns0.906 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 140 %140 %ASTM D882
Film Elongation at Break, TD 80 %80 %ASTM D882
Modulus of Elasticity 3.79 GPa550 ksi(stiffness), ASTM D882
Tear Strength Test 500500Graves, g; ASTM D1004
Film Tensile Strength at Break, MD 187 MPa27100 psiASTM D882
Film Tensile Strength at Break, TD 276 MPa40000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FMay be used to contain foods during baking above this temperature.
Shrinkage, MD 1.6 %
@Temperature 150 °C,
Time 1800 sec
1.6 %
@Temperature 302 °F,
Time 0.500 hour
Film shrinkage in oven.
Shrinkage, TD 1.6 %
@Temperature 150 °C,
Time 1800 sec
1.6 %
@Temperature 302 °F,
Time 0.500 hour
Film shrinkage in oven.
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM D1003
Gloss 150 %150 %20°; ASTM D2457
Transmission, Visible 70 %70 %% Clarity; ASTM D1746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil C4LL 20025.17 Linear Low Density Polyethylene Resin
ExxonMobil LL 6100 Injection Molding Resin
Tabriz LL 0410AA Low Density Polyethylene copolymer
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
ExxonMobil C4LL 1018.76 Linear Low Density Polyethylene Resin

PDU658 / 33107

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.