MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eurotec® Tecomid® NB50 NL IT PA 6 super tough
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes:
  • Excellent stiffness/toughness balance
  • High mechanical strength
  • Very good thermal stability
  • Excellent flammability characteristics
  • Good electrical properties
  • High wear resistance and low friction
  • Very good chemical resistance
  • Good flow and processing properties

APPLICATIONS:

  • Automotive
  • Electrical/Electronic
  • Furniture
  • Construction
  • Home appliances

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Filler Content 0.00 %0.00 %ISO 3451
Moisture Absorption at Equilibrium 2.2 %2.2 %Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 8.0 %8.0 %23°C; ISO 62
Linear Mold Shrinkage 0.014 cm/cm0.014 in/in
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 200 %200 %ISO 527
Izod Impact, Notched (ISO)  30.0 kJ/m²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 95.0 kJ/m²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched  3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/eA
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °F10 K/min; ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/2
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond NYLON 6615 Black, Super Tough
DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI
E-Polymers TEKAMID® TB120ST Super Tough PA6, DAM
E-Polymers TEKAMID® TA210ST Super Tough PA66, DAM
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)

PEUROT24 / 37254

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.