MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek StatSafe™ ADC Static Dissipative Alumina
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffness, wear and corrosion resistance, low thermal expansion, and dimensional stability. Typical applications include: end effectors, ESD sensitive component handling, data storage drive components, and data storage drive manufacturing tools.

Key Words: Al2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.85 g/cc0.139 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 370 GPa53700 ksi
Flexural Strength 300 MPa43500 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 - 1.00e+7 ohm-cm1.00e+6 - 1.00e+7 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C4.44 µin/in-°F
Thermal Conductivity 25.0 W/m-K174 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum A360.0-F Die Casting Alloy
Aluminum 384.0-F Die Casting Alloy
Aluminum 380.0-F Die Casting Alloy
Aluminum A380.0-T5, Casting Alloy
Aluminum 514.0-F, Sand Cast

CCOOR915 / 104619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.