MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchcast™ 2123 Re-enterable Insulating Electrical Resin
Categories: Polymer; Thermoset

Material Notes: 3M Scotchcast Re-enterable Electrical Resin 2123 is a soft, two-part polybutadine resin encapsulant designed especially for re-enterable splice protection. It is formulated for virtually every electrical application requiring a soft, re-enterable resin with good handling and performance characteristics. This resin is also used as the insulating material for cable splicing operating at 1000 volts and is rated for continuous use at 90°C with an overload rating of 130°C. It may be stocked to cover most re-enterable resin needs, ending the need for multiple encapsulant inventories. Scotchcast Resin 2123 is formulated with excellent wetting properties and low viscosity. The resin flows well even at low temperatures, filing the closure and minimizing voids.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.0738 MPa10.7 psiASTM D412
Elongation at Break 300 %300 %ASTM D412
Tear Strength 0.280 kN/m1.60 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 4.00e+11 ohm>= 4.00e+11 ohmMS 17000, Section 1182
Dielectric Constant >= 1.2
@Frequency 100 Hz
>= 1.2
@Frequency 100 Hz
ASTM D150
Dielectric Strength >= 9.45 kV/mm
@Thickness 3.17 mm
>= 240 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.00080
@Frequency 100 Hz
0.00080
@Frequency 100 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °FContinuous
 130 °C266 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 21.0 °C
24.0 hour
@Temperature 69.8 °F
Gel Time 62.0 min62.0 min
 
Descriptive Properties
AppearanceAmber Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate
Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems
Covestro Bayblend® KL 1-1430 Polycarbonate/ABS Blend
Master Bond MasterSil 415 One Component Room Temperature Curing, Transparent Silicon

PMM35239 / 169986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.