MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Atom Adhesives AA-DUCT 916 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-DUCT 916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good electrical and mechanical properties. AA-DUCT 916 is two-part, smooth paste adhesive of refined pure silver and epoxy resin components. It is free of solvents and copper or carbon additives. It develops strong, durable, resilient, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic insulates. AA-DUCT 916 cures at room temperature and can be used as a flexible "cold-solder" for heat-sensitive components where hot-soldering is impractical. It also can be used for the assembly and repair of electrical modules, flexible circuits, wave guides, flat cable and high frequency shields.

Appearance: Silver

Cure Type: Heat cure or Room temperature

Mix Ratio by weight: 100:115/Resin:Hardener

Benefits:

  • High strength
  • Perfect bond
  • Cold solder for heat sensitive components
Substrates: Excellent choice aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards.

Typical Application: It can be used as a flexible "cold-solder" for heat-sensitive components where hot-soldering is impractical. The assembly and repair of electrical modules, flexible circuits, wave guides, flat cable and high frequency shields.

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.85 g/cc2.85 g/ccuncured
Solids Content 100 %100 %reactive, uncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464cured
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00010 ohm-cm<= 0.00010 ohm-cmcured
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 110 °C230 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 5.00 °C41.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 240 min
@Temperature 65.0 °C
1.00 - 4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 180 min180 minuncured
Shelf Life 12.0 Month12.0 Monthuncured
 
Descriptive Properties
ViscosityPasteuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Duct 2956 Low Ion Snap Cure Silver Epoxy Adhesive
Aremco Aremco-Bond™ 556-HT-HC Electrically & Thermally Conductive Adhesive, Silver-Filled, Highly Conductive
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative
Overview of materials for Epoxy, Electrically Conductive
Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive

PATOM048 / 172363

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.