MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Sheet and Strip, UNS N07718
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to approximately 982 degrees Celsius. In addition, the alloy exhibits excellent tensile and impact strength even at cryogenic temperatures. High strength at room and elevated temperatures is developed by a precipitation heat treatment at 718 degrees Celsius with cooling and a hold at 621°C.

The relatively slow response to precipitation hardening permits repair welding of the Altemp 718 alloy even in the aged condition. The Altemp 718 alloy is usually produced by a double melt practice using consumable electrode remelt procedures to provide homogeneity and extremely clean structures. Specific uses include aircraft ducting and engine plumbing.

Tensile properties below are from AMS 5596 and/or AMS 5597.

Information provided by Allegheny Ludlum

Key Words: DIN 2.4668; ASTM B-670; AMS 5596; AMS 5597
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.19 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9595Typical Annealed
Tensile Strength, Ultimate <= 965 MPa<= 140000 psi
Tensile Strength, Yield <= 550 MPa
@Strain 0.2 %
<= 79800 psi
@Strain 0.2 %
Elongation at Break >= 30 %>= 30 %in 2"
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.2940.294
Shear Modulus 77.0 GPa11200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000127 ohm-cm0.000127 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.8 µm/m-°C
@Temperature 20.0 - 93.0 °C
7.11 µin/in-°F
@Temperature 68.0 - 199 °F
 13.9 µm/m-°C
@Temperature 20.0 - 315 °C
7.72 µin/in-°F
@Temperature 68.0 - 599 °F
 14.4 µm/m-°C
@Temperature 20.0 - 538 °C
8.00 µin/in-°F
@Temperature 68.0 - 1000 °F
Thermal Conductivity 11.2 W/m-K
@Temperature 0.000 - 100 °C
77.7 BTU-in/hr-ft²-°F
@Temperature 32.0 - 212 °F
Maximum Service Temperature, Air 982 °C1800 °Foxidation resistance to this temp
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.50 %0.50 %
Boron, B 0.0030 %0.0030 %
Carbon, C 0.050 %0.050 %
Chromium, Cr 18.5 %18.5 %
Cobalt, Co 0.30 %0.30 %
Copper, Cu 0.050 %0.050 %
Iron, Fe 18 %18 %as balance
Manganese, Mn 0.10 %0.10 %
Molybdenum, Mo 3.0 %3.0 %
Nickel, Ni 53 %53 %
Niobium, Nb (Columbium, Cb) 5.1 %5.1 %
Phosphorus, P 0.0060 %0.0060 %
Silicon, Si 0.15 %0.15 %
Sulfur, S 0.0010 %0.0010 %
Titanium, Ti 1.0 %1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 718
ATI Allvac® 718 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age
ATI Allvac® 718-OP® UNS N07718 Nickel Superalloy
Haynes 718 alloy, cold rolled, solution-treated and aged sheet
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy

NLN71A / 18021

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.