MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic Adhesive
Lord 660 Acrylic Adhesive bonds FRP (fiber-reinforced plastics) with minimal surface preparation. Lord 660 can cross-bond FRP to many metals. This adhesive is specifically formulated to produce the highest impact and peel strengths available in a room temperature curing adhesive.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 - 1.02 g/cc0.0351 - 0.0368 lb/in³
Viscosity 10000 - 80000 cP10000 - 80000 cPHardener
 
Thermal PropertiesMetricEnglishComments
Flash Point 15.0 °C59.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour
Pot Life 20 - 40 min20 - 40 minTime before parts must be mated
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles
Polyimide Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge
Honeywell Spectra® 900 Fiber

PLORDAD13 / 51995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.