MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemical Concepts Chem-Set™ 711 Fast Set Hot Melt Adhesive
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Hot melt adhesive for packaging and sealing cartons for medium to larger cartons. This adhesive has an excellent hot tack for fast and strong bond. Will bond to most porous materials including wood. Compositional compliance with FDA Regulation #21CFR175.105 for food packaging. Suggested Uses: Packaging adhesive with excellent hot tack, short open time and good delivery rate. Good adhesion to plain and some coated corrugated packaging and paper products. Fast Set. Precautions: Do Not Mix with other adhesives. Severe burns will result if contact is made in molten state. Material safety data sheets provide safety precautions that should be observed in handling and storing.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity  3800 cP
@Temperature 375 °C
3800 cP
@Temperature 707 °F
 7400 cP
@Temperature 325 °C
7400 cP
@Temperature 617 °F
Brookfield Viscosity 24000 cP
@Temperature 250 °C
24000 cP
@Temperature 482 °F
spindle SC4-27; ASTM D3236
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °FPeel Adhesion Failure. ASTM D4498, 45# Kraft paper substrates, 500 g weights.
Flash Point >= 232 °C>= 450 °F
Shear Adhesion Failure Temperature 78.9 °C174 °F45# Kraft paper substrates, 500 g weights.; ASTM D4498
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 193 °C>= 380 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Colortan
Mettler Softening Point208°F, ASTM D6493-99
Odormoderate
Open Time10 seconds, using 45# Kraft paper substrates, ASTM D4497-94 (1999)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay BR® 127 Primer with FM 73 Adhesive
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
American Pine Wood
Chemical Concepts Chem-Set™ 738 General Purpose Hot Melt Adhesive
Northern White Pine Wood

PCHEMI924 / 232172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.