MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond MasterSil 151AN Silicone Features High Thermal Conductivity
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Master Bond MasterSil 151AN is a two component, low viscosity silicone compound for high performance potting and encapsulation. This system combines high temperature resistance, good flexibility, thermal conductivity and electrical insulation properties. It is an addition cured system and does not require exposure to air for complete cross-linking. It has a 100 to five mix ratio by weight. It is 100% solids, contains no solvents or diluents and will not outgas while curing. MasterSil 151AN system is a low viscosity making it highly desirable for potting and encapsulation. As a silicone system, it offers excellent flexibility and high temperature resistance. Its flexibility allows it to withstand severe thermal cycling and resist vibration and shock. Also, it is very water resistant. These properties make this system well suited for applications involving sensitive optical and electronic components where heat dissipation is critical. Some additional applications include heat sink attachment, potting sensors and thermocouple applications, among many other uses. MasterSil 151AN is gray in color. The service temperature range for this system is -65°F to +400° F.

Product Advantages:

  • Addition cured; no by-products released during cure; does not require air for curing.
  • Low exotherm; very long pot life.
  • Readily cures at ambient temperatures or faster cure at elevated temperatures.
  • Can cure in thicknesses up to and beyond 1-2 inches.
  • Very low shrinkage upon cure.
  • Low viscosity ideal for potting and encapsulation.
  • Superior electrical insulation properties.
  • Outstanding flexibility combined with high temperature resistance and very good thermal conductivity.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 50 - 150 cP50 - 150 cPPart B
 17000 - 240000 cP17000 - 240000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75 - 8575 - 85
Tensile Strength at Break 5.52 - 6.21 MPa800 - 900 psi
Elongation at Break 120 - 150 %120 - 150 %
Shear Strength >= 0.276 MPa>= 40.0 psiBond, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Constant 2.7
@Frequency 100 Hz,
Temperature 25.0 °C
2.7
@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 17.7 kV/mm
@Thickness 3.17 mm
450 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 - 150 µm/m-°C66.7 - 83.3 µin/in-°F
Thermal Conductivity 3.17 - 3.46 W/m-K22.0 - 24.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Pot Life 2.0 - 4.0 min2.0 - 4.0 min100 gram batch
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)100:50by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 151AO Thermally Conductive Silicone System
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond MasterSil 151 Two Component Low Viscosity Silicone Compound
Master Bond EP110F6 Thermal Shock Resistant, Electrically Insulating Epoxy
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System

PMASTB333 / 149580

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.