MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Magnesium AZ61A-F, Extruded Hollow Shapes
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Similar to but stronger than AZ31B-F.

Key Words: UNS M11610; Mg
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 5050500 kg load, 10 mm ball
Tensile Strength, Ultimate 280 MPa40600 psi
Tensile Strength, Yield 165 MPa23900 psi
Elongation at Break 14 %14 %in 50 mm
Tensile Modulus 45.0 GPa6530 ksi
Compressive Yield Strength 110 MPa16000 psi
Poissons Ratio 0.350.35
Fatigue Strength 125 - 160 MPa
@# of Cycles 1.00e+8
18100 - 23200 psi
@# of Cycles 1.00e+8
R.R. Moore Test
Machinability 100 %100 %Relative Rating, 100=Best
Shear Modulus 17.0 GPa2470 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000125 ohm-cm0.0000125 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 370 J/g159 BTU/lb
CTE, linear  26.0 µm/m-°C
@Temperature 0.000 - 100 °C
14.4 µin/in-°F
@Temperature 32.0 - 212 °F
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
15.0 µin/in-°F
@Temperature 68.0 - 392 °F
Estimated from similar Mg alloys
Specific Heat Capacity 1.05 J/g-°C0.251 BTU/lb-°F
Thermal Conductivity 70.0 W/m-K486 BTU-in/hr-ft²-°FEstimated from trends in similar Mg alloys.
Melting Point >= 418 °C>= 784 °FIncipient Melting
Solidus 525 °C977 °F
Liquidus 620 °C1150 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 400 °C446 - 752 °FHot Working
Annealing Temperature 345 °C653 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.8 - 7.2 %5.8 - 7.2 %
Copper, Cu <= 0.050 %<= 0.050 %
Iron, Fe <= 0.0050 %<= 0.0050 %
Magnesium, Mg 92 %92 %As Remainder
Manganese, Mn >= 0.15 %>= 0.15 %
Nickel, Ni <= 0.0050 %<= 0.0050 %
Silicon, Si <= 0.10 %<= 0.10 %
Zinc, Zn 0.40 - 1.5 %0.40 - 1.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AZ61A-F, Extruded Solid Shapes
Magnesium Elektron AZ61 Magnesium Alloy
Magnesium AS41A-F, Die Cast
Magnesium AZ61A-F, Forgings
Magnesium AZ80A-T5, Extruded

MMAZ60 / 12320

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.