MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Thornel® VCB-20 Carbon Fiber Cloth  (discontinued **)
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Used as a reinforcement in structural, ablative, and abrasion-resistant composites.

2000 filaments/strand, 99+% carbon assay

Solvay has acquired the Thornel product line as a part of the Cytec purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.88 g/cc0.0679 lb/in³Fiber Density
Specific Surface Area 1.0 m²/g1.0 m²/g
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1380 MPa200000 psiFiber Strand
Tensile Modulus 138 GPa20000 ksiFiber strand
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.710 J/g-°C0.170 BTU/lb-°F
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FAcross ply
 15.0 W/m-K104 BTU-in/hr-ft²-°FFiber Value

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
Solvay Thornel® Mat VMA Carbon Fiber
Solvay Thornel® VCB-20 Carbon Cloth/Epoxy Composite
Momentive Performance Materials "PG" Pyrolytic Graphite
Pyrolytic Graphite, Low Temperature Isotropic (LTI)

ETHORQ / 6098

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.