MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

DSM Somos® NanoTool™ Resin for Stereolithography, UV & Thermal Postcure
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: NanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavily filled with non-crystalline nanoparticles allowing for faster processing. It exhibits superior side wall quality, along with excellent detail resolution as compared to other composite stereolithography materials.

Application

NanoTool's smooth surface quality and high initial modulus make it an excellent resin for metal plating, a growing application which saves time and money as an alternative to fully metal prototypes. It's also ideal for creating strong, stiff parts that need to resist high temperatures, including wind tunnel models for aerospace and automotive applications. A third major application area is rapid tooling for injection molding.

Information Provided by DSM Desotech Inc.

Key Words: Third Generation ProtoComposite™ Material for High Strength, High Temperature Applications
Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. North American leaders in delivering quick turnaround Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including SLA Stereolithography prototypes. Free online 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc
@Temperature 25.0 °C
0.0596 lb/in³
@Temperature 77.0 °F
Water Absorption 0.15 - 0.16 %0.15 - 0.16 %ASTM D570-98
Viscosity 2500 cP
@Temperature 30.0 °C
2500 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9494ASTM D2240
Tensile Strength, Yield 66.3 - 80.3 MPa9620 - 11600 psiASTM D638M
Elongation at Break 0.70 - 1.0 %0.70 - 1.0 %ASTM D638M
Tensile Modulus 10.4 - 11.2 GPa1510 - 1620 ksiASTM D638M
Flexural Strength 103 - 149 MPa14900 - 21600 psiASTM D790M
Flexural Modulus 9.96 - 10.2 GPa1440 - 1480 ksiASTM D790M
Poissons Ratio 0.29 - 0.360.29 - 0.36ASTM D638M
Izod Impact, Notched 0.140 - 0.160 J/cm0.262 - 0.300 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
ASTM D150-98
 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
ASTM D150-98
 3.9
@Frequency 60.0 Hz
3.9
@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 16.1 - 16.9 kV/mm409 - 429 kV/inASTM D149-97a
 
Thermal PropertiesMetricEnglishComments
CTE, linear  25.0 - 25.7 µm/m-°C
@Temperature -40.0 - 0.000 °C
13.9 - 14.3 µin/in-°F
@Temperature -40.0 - 32.0 °F
ASTM E831-00
 25.5 - 31.3 µm/m-°C
@Temperature 0.000 - 50.0 °C
14.2 - 17.4 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831-00
 57.0 - 58.9 µm/m-°C
@Temperature 50.0 - 100 °C
31.7 - 32.7 µin/in-°F
@Temperature 122 - 212 °F
ASTM E831-00
 95.2 - 99.6 µm/m-°C
@Temperature 100 - 150 °C
52.9 - 55.3 µin/in-°F
@Temperature 212 - 302 °F
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 258 - 263 °C496 - 505 °FASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FASTM D648-98c
Glass Transition Temp, Tg 86.0 - 89.0 °C187 - 192 °FASTM E1545-00
 
Descriptive Properties
AppearanceOff White
Dp (mm)0.11Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2)84Exposure that gives 0.254mm thickness
Ec (mJ/cm2)8.3Critical exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV & Thermal Postcure
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2

PDSMT013 / 93533

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.