MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Moplen EP500N Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen EP500N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP500N is a block copolymer particularly suitable for injection molding of containers, parts of electrical appliances, crates and pails. Moplen EP500N meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520. And the components of additives are adequate on the food packaging substances specification of FDA regulation 21 CFR 178.2010.

Features: Optimized balance of stiffness and toughness; High impact strength even at low temperature; Narrow molecular weight distribution; Low warpage; High whiteness; High gloss

Applications: Parts of electrical appliances; Pail; Housewares; Furniture (Chairs)

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ASTM D785
Tensile Strength, Yield 26.5 MPa3840 psiASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus 1.13 GPa164 ksiASTM D790
Izod Impact, Notched  0.490 J/cm
@Temperature -20.0 °C
0.918 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.981 J/cm
@Temperature 23.0 °C
1.84 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen EP300R Injection Molding Grade Polypropylene
PolyMirae Moplen EP300H Injection Molding Grade Polypropylene
PolyMirae Moplen 342R Injection Molding Grade Polypropylene
PolyMirae Moplen EP640V Injection Molding Grade Polypropylene
PolyMirae Moplen EP540T Injection Molding Grade Polypropylene

PMIRAE15 / 53127

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.