MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Momentive Performance Materials Silopren™ LSR 4640 Liquid Silicone Rubber - Healthcare
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding process allows for complex part geometry and exact dimensions. LSR elastomers are generally suitable for short cycle time injection and full automatic flash-less processing. Color pastes are available to pigmenting addition cure productions of LSR's.

All LSR grades are platinum cured materials which are mixed in a 1:1 ratio by weight.

The distinctive properties of silicone elastomers - purity, clarity, strength - coupled with ease of processability, have resulted in their use in a broad range of medical device applications. Silicone materials exhibit exceptional stability over a wide range of temperatures, lending themselves to use in applications requiring repeated sterilization performance.

Typical applications include, but are not limited to:

  • Dental / surgical devices
  • Diagnostics / imaging
  • Fluid and drug delivery devices
  • Orthopedics / prosthetics
  • Scar management
  • Septa / stoppers / laboratory accessories
  • Medical tubing
  • Wound drains and bulbs
  • Sterilization mats
  • Pharmaceutical closures
  • Instrument grips
  • Dialysis o-rings
  • Positioning devices
  • Catheters
  • Seals / o-rings / valves
  • Respiratory / anesthesia
  • Medical equipment keypads

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
Linear Mold Shrinkage 0.027 cm/cm0.027 in/invulcanized 10 sec at 200°C; Without post-cure
 0.035 cm/cm0.035 in/invulcanized 10 sec at 200°C then post-cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4242
Tensile Strength 8.00 MPa1160 psi
Elongation at Break 600 %600 %
Tear Strength 45.0 kN/m257 pliDie B
Compression Set 25 %25 %Post cured
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 %80 %transparent; thickness unknown
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 20.0 °C68.0 °Fcool nozzle and cylinder to prevent premature vulcanization
Mold Temperature 140 - 230 °C284 - 446 °Fshort vulcanization time required (a few seconds)
Injection Pressure 5.00 - 15.0 MPa725 - 2180 psidepends on feed channel
Hold Pressure 5.00 MPa725 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600
USP Class VI YesYesUSP Class VI methods: Intramuscular implantation, intracutaneous injection, & systematic injection
 
Descriptive Properties
AppearanceTransparent
BfRproduct is compositionally compliantRecommendation XV Silicones; post cured (4h/200°C)
ISO10993yes7 ISO 10993 tests applicable to "wet" chemicals

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil MED-4080 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use
Momentive Performance Materials TSE 2287U Heat Cured Rubber - High Duro Translucent
Momentive Performance Materials Addisil™ 482 E Healthcare Extrusion Grade Heat Cured Rubber
Momentive Performance Materials Addisil™ 1140 M Industrial Molding Heat Cured Rubber
Dow Silastic® Q7-4750 BIOMEDICAL GRADE ETR ELASTOMER, KIT

PGE8V751 / 109011

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.