MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baypreg® F Polyurethane, Natural Fiber Glass
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baypreg F system is a two component polyurethane system used in compression molding.

Properties / Applications: Baypreg F system is a two component polyurethane system used in compression molding of natural fiber mats alone, or fiber-reinforced sandwich panels to produce a variety of automotive parts. Some identified applications include door panels, sunshades, spare tire covers, load floors, etc. The Baypreg F system provides lightweight alternatives to ABS, PP, SMC, and wood products while demonstrating very high flexural stiffness and excellent thermal properties. Baypreg F system offers very diverse properties over a wide range of part thicknesses and densities while still providing cost effective substrate parts when combined with reinforcing materials. As with any product, use of the Baypreg F system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.800 g/cc0.800 g/ccASTM D792
 1.05 g/cc1.05 g/ccPolyol Blend (Component B)
 1.21 g/cc1.21 g/ccIsocyanate (Component A)
Viscosity 350 cP350 cPIsocyanate (Component A)
 800 cP800 cPPolyol Blend (Component B)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.0 MPa2470 psiASTM D638
Flexural Strength 17.0 MPa2470 psiASTM D790
Flexural Modulus 3.70 GPa537 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.6 µm/m-°C17.0 µin/in-°FASTM D696
Flash Point 160 °C320 °FPolyol Blend (Component B)
 223 °C433 °FIsocyanate (Component A)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 100 - 120 °C212 - 248 °F
 
Descriptive Properties
AppearanceBlack liquidPolyol Blend (Component B)
 Dark brown liquidIsocyanate (Component A)
Content28.5%NCO, Isocyanate (Component A)
Hydroxyl number[KOH/g], Polyol Blend (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kareline Oy PPMS5050 Natural Fiber Reinforced Polypropylene for injection molding
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber
Polynt BMC 580 Bulk Molding Compound Green Compound With Natural Fiber

PCOVEST0216 / 201999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.