MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

317 Stainless Steel, Cold finished bar
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Key Words: UNS S31700, AISI 317, DIN 1.4449, DIN X5CrNiMo1713, ASTM A 276 A276
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  515 MPa
@Diameter >=12.7 mm
74700 psi
@Diameter >=0.500 in
 620 MPa
@Diameter <=12.7 mm
89900 psi
@Diameter <=0.500 in
Tensile Strength, Yield  205 MPa
@Diameter >=12.7 mm
29700 psi
@Diameter >=0.500 in
 310 MPa
@Diameter <=12.7 mm
45000 psi
@Diameter <=0.500 in
Elongation at Break  30 %
@Diameter >=12.7 mm
30 %
@Diameter >=0.500 in
 30 %
@Diameter <=12.7 mm
30 %
@Diameter <=0.500 in
Reduction of Area  40 %
@Diameter >=12.7 mm
40 %
@Diameter >=0.500 in
 40 %
@Diameter <=12.7 mm
40 %
@Diameter <=0.500 in
Modulus of Elasticity 195 GPa28300 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000740 ohm-cm0.0000740 ohm-cmat 20ºC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.0 µm/m-°C
@Temperature 0.000 - 100 °C
8.89 µin/in-°F
@Temperature 32.0 - 212 °F
 16.2 µm/m-°C
@Temperature 0.000 - 315 °C
9.00 µin/in-°F
@Temperature 32.0 - 599 °F
 17.5 µm/m-°C
@Temperature 0.000 - 540 °C
9.72 µin/in-°F
@Temperature 32.0 - 1000 °F
Specific Heat Capacity 0.502 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
113 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point 1370 - 1400 °C2500 - 2550 °F
Solidus 1370 °C2500 °F
Liquidus 1400 °C2550 °F
Maximum Service Temperature, Air 870 °C1600 °FIntermittent
 925 °C1700 °FContinuous Service
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe 57.85 - 68 %57.85 - 68 %As Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 3.0 - 4.0 %3.0 - 4.0 %
Nickel, Ni 11 - 15 %11 - 15 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
317 Stainless Steel, Hot finished and annealed bar, forgings
317 Stainless Steel, annealed plate
317 Stainless Steel, Annealed Bar
317 Stainless Steel, annealed sheet
317 Stainless Steel, annealed strip

MQ317De / 171834

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.