MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type M1 Molybdenum-Alloy High-Speed-Tool Steel (UNS T11301)
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Fe-8.7Mo-3.75Cr-1.25W-1.15V-0.8C

Key Words: UNS T11301
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 60 - 6560 - 65
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.1 µm/m-°C5.61 µin/in-°F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 540 - 595 °C1000 - 1100 °FTempering Temperature
 1175 - 1220 °C2147 - 2230 °FHardening Temperature
Annealing Temperature 815 - 870 °C1500 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.80 %0.80 %
Chromium, Cr 3.75 %3.75 %
Iron, Fe 84.3 %84.3 %As Balance
Molybdenum, Mo 8.7 %8.7 %
Tungsten, W 1.25 %1.25 %
Vanadium, V 1.15 %1.15 %
 
Descriptive Properties
Quench MediumO, A, S

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M10 Molybdenum High Speed Tool Steel (UNS T11310)
AISI Type M3 Class 1 Molybdenum High Speed Tool Steel (UNS T11313)
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
AISI Type T1 Tungsten-Alloy High-Speed-Tool Steel (UNS T12001)
AISI Type M4 Molybdenum High Speed Tool Steel (UNS T11304)

MSTM1 / 100271

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.