MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Quartz-Coat™ 845-D / 845-S High Temperature Specialty Coatings Inorganic, Silicon Filled  (discontinued **)
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Ceramic-metallic, dark gray diffusion coating for quartz lamp applications to 2000 °F. Used mainly for coating automotive headlamps and stadium lighting. Refer to dip and spray formulations as Quartz-Coat™ 845-D (dip) and 845-S (spray). Now available in opaque blue as 845-Blue. Other colors available upon request.

Vendors: Aremco offers a wide range of ceramic, glass and silicone based coatings for ceramic, glass and quartz materials used in heater and lighting applications to 2000°F (1093°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc1.55 g/cc
Solids Content 42 %42 %by volume
 55 %55 %by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Viscosity 400 - 700 cP400 - 700 cP
Thickness 33.0 microns1.30 milrecommended dry film thickness
 76.2 microns3.00 milestimated wet film thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1090 °C2000 °FContinuous
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Dry Time 0.5 hour0.5 hourHandling
 0.1 - 1 hour0.1 - 1 hourRecoat
Cure Time >= 3.00 min>= 0.0500 hourAir Set prior to curing
 12.0 min0.200 hour0.1 hr at 200°F; 0.1 hr at 900°F
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Dry Film Coverage ft2/gal630at 1 mil
ThinnerDistilled Water

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5878 Additive
Titanium Aluminum Nitride (TiAlN) PVD Coating
Evonik BREAK-THRU® S 240 Surfactants
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating

ZCAREM37 / 578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.