MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUTENE-H BE0400 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.

Applications: Blow molded containers with capacities ranging a few milliliters up to 20 liters, Sheet

CAS No. 9002-88-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.957 g/cc0.957 g/ccASTM D792
Environmental Stress Crack Resistance 50 hour50 hourF50; ASTM D1693
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240
Tensile Strength, Yield 30.4 MPa
@Thickness 3.20 mm
4410 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break >= 600 %
@Thickness 3.20 mm
>= 600 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Modulus 1.37 GPa199 ksi15mm/min; ASTM D790
Izod Impact, Notched 2.45 J/cm
@Thickness 6.40 mm,
Temperature 20.0 °C
4.59 ft-lb/in
@Thickness 0.252 in,
Temperature 68.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °FDSC
Brittleness Temperature <= -80.0 °C<= -112 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Adapter Temperature 180 °C356 °FIdeal, Extrusion Blow Molding
 180 - 190 °C356 - 374 °FExtrusion Blow Molding
Die Temperature 170 °C338 °FIdeal, Extrusion Blow Molding
 160 - 190 °C320 - 374 °FExtrusion Blow Molding
Melt Temperature 180 °C356 °FIdeal, Extrusion Blow Molding
 180 - 200 °C356 - 392 °FExtrusion Blow Molding
 
Descriptive Properties
Barrel160-185°CIntake Zone, Extrusion Blow Molding
 165°CIntake Zone, Ideal, Extrusion Blow Molding
 175-195°CCompression Zone, Extrusion Blow Molding
 180°CCompression Zone, Ideal, Extrusion Blow Molding
 180-200°CMetering Zone, Extrusion Blow Molding
 190°CMetering Zone, Ideal, Extrusion Blow Molding
Cross Head165-195°CExtrusion Blow Molding
 180°CExtrusion Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUTENE-H ME6000 HDPE
LG Chemical LUTENE-H ME2500 HDPE
LG Chemical LUTENE-H ME8000 HDPE
LG Chemical LUTENE-H BE0350 HDPE
LG Chemical LUTENE-H ME1000 High Density Polyethylene

PLAY194 / 148204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.