MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Johnson Matthey Silver-flo™ 56 Cadmium Free Silver Brazing Paste
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silver-flo™ 56 Brazing Paste is a custom made solution for improving the quality and production rate of brazing operations. It consists of Silver-flo™ 56 powder, a cadmium-free silver brazing filler metal, combined with a flux-binder system to form a smooth dispensable paste.

The use of a brazing paste provides the opportunity for automation or semi-automation of the brazing process by de-skilling and allowing pre-placement of the brazing material. It reduces handling, waste and can improve joint quality by helping to provide repeatability in brazing.

The filler metal, Silver-flo™ 56, combines a low brazing temperature with a short melting range is very free flowing and produces neat joints with small fillets. These characteristics make Silver-flo™ 56 an excellent general-purpose silver brazing filler metal.

Silver-flo™ 56 Brazing Paste is an extremely versatile product and has been used in a range of diverse applications from the brazing of electrical contacts, to pipes in musical instruments or the tubes and brackets in shot guns for example.

Silver-flo™ 56 can be used to join all the common engineering materials (excluding aluminum) such as copper, copper alloys (including, brasses, bronzes, gun metal, nickel silvers, aluminum bronze, copper nickel), steels including, mild, carbon, tool steel, stainless steels, low alloy steel), tungsten carbide and PCD segments. On large or difficult to wet tungsten carbide pieces specialized silver brazing filler metals containing nickel / manganese are often preferred.

Paste Grades: 106-B1-70, 180-B1-75

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 618 - 652 °C1140 - 1210 °F
Solidus 618 °C1140 °F
Liquidus 652 °C1210 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 22 %22 %
Silver, Ag 56 %56 %
Tin, Sn 5.0 %5.0 %
Zinc, Zn 17 %17 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey Argo-braze 49H Silver Brazing Alloy for Tungsten Carbide Brazing
Johnson Matthey Silver-flo™ 452 Cadmium Free Silver Brazing Filler Metal
Johnson Matthey D Bronze High Temperature Alloy for Tungsten Carbide Brazing
Johnson Matthey Argo-braze™ 502 Tri-foil Silver Brazing Filler Metal
Johnson Matthey Silver-flo™ 56 Cadmium Free Silver Brazing Filler Metal

NJMMJ9769 / 186170

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.