MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Neodymium® 27H Hard Magnetic Alloy
Categories: Metal; Electronic/Magnetic Alloy

Material Notes: NdFeB

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.40 g/cc0.267 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cm
Magnetic Coercive Force, Hc 9789 Oe9789 Oe
Magnetic Remanence, Br 10800 Gauss10800 Gauss
Magnetic Maximum Energy Product, BH 27.02 MGOe27.02 MGOe
Curie Temperature 300 °C572 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 - 8.00 µm/m-°C2.78 - 4.44 µin/in-°F
Maximum Service Temperature, Air 100 °C212 °F
 
Descriptive Properties
Intrinsic Magnetic Coercive Force, HCi (Oe)17002

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Neodymium® 27 Hard Magnetic Alloy
Neodymium® 30 Hard Magnetic Alloy
Neodymium® 30H Hard Magnetic Alloy
Chromindur® II Hard Magnetic Alloy
Alnico® 8HC (Anisotropic, Sintered) Hard Magnetic Alloy

MM918 / 100433

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.