MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cast Stainless Steel HK, ASTM A297
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel

Material Notes: Austenitic, heat resistant

Key Words: ASTM A297/A297M(98)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 450 MPa>= 65300 psi
Tensile Strength, Yield >= 240 MPa>= 34800 psi
Elongation at Break >= 10 %>= 10 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.20 - 0.60 %0.20 - 0.60 %
Chromium, Cr 24 - 28 %24 - 28 %
Iron, Fe 44.8 - 57.8 %44.8 - 57.8 %As remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni 18 - 22 %18 - 22 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 2.0 %<= 2.0 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Stainless Steel HX, ASTM A297
MetalTek MTEK HK40 Cast UNS J94204 Heat Resistant Stainless Steel
ASTM A36 Steel, plate
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel
Cast Stainless Steel HK, ACI

MQCHK0030 / 13435

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.