MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® LED2245 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: MVR (300 °C/1.2 kg) 34 cm³/10 min; light guides; optics and lenses; PC with highest transmission; low viscosity; easy release; injection molding - melt temperature 280 - 320 °C

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.660 g/cc0.0238 lb/in³pellets; ISO 60
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.12 %0.12 %ISO 62
Water Absorption at Saturation 0.30 %0.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0065 cm/cm0.0065 in/in60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 37 g/10 min
@Load 1.20 kg,
Temperature 300 °C
37 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 115 MPa16700 psi² ISO 2039-1
Tensile Strength at Break 60.0 MPa8700 psi50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 63.0 MPa9140 psi50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, 50 mm/min; ISO 527-1/-2
 125 %125 %50 mm/min; ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2.35 GPa341 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 97.0 MPa14100 psi2 mm/min; ISO 178
Flexural Yield Strength 73.0 MPa
@Strain 3.5 %
10600 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.35 GPa341 ksi2 mm/min; ISO 178
Flexural Strain at Yield 7.1 %7.1 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  1.20 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
0.571 ft-lb/in²
@Thickness 0.118 in,
Temperature -22.0 °F
complete break; ISO 7391/b.o. ISO 180-A
 55.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
26.2 ft-lb/in²
@Thickness 0.118 in,
Temperature 73.4 °F
partial break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature -60.0 °C
NB
@Temperature -76.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Thickness 3.00 mm,
Temperature -30.0 °C
5.71 ft-lb/in²
@Thickness 0.118 in,
Temperature -22.0 °F
complete break; ISO 7391/b.o. ISO 179-1eA
 6.00 J/cm²
@Thickness 3.00 mm,
Temperature 23.0 °C
28.6 ft-lb/in²
@Thickness 0.118 in,
Temperature 73.4 °F
partial break; ISO 7391/b.o. ISO 179-1eA
Impact 49004900Puncture - maximum force (N); ISO 6603-2
 5900
@Temperature -30.0 °C
5900
@Temperature -22.0 °F
Puncture - maximum force (N); ISO 6603-2
Puncture Energy 55.0 J40.6 ft-lbISO 6603-2
 60.0 J
@Temperature -30.0 °C
44.3 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm864 kV/in1 mm; IEC 60243-1
Dissipation Factor  0.00050
@Frequency 100 Hz
0.00050
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VCIT M; Solution B; IEC 60112
 250 V250 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°Fcross-flow; ISO 8302
Hot Ball Pressure Test 136 °C277 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °C280 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FISO 75-1/-2
Vicat Softening Point 145 °C293 °F50°C/h 50N; ISO 306
 146 °C295 °F120°C/h 50N; ISO 306
Glass Transition Temp, Tg 145 °C293 °FISO 11357-1/-2
UL RTI, Electrical 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
IEC 60695-11-10
 V-2
@Thickness 2.90 mm
V-2
@Thickness 0.114 in
IEC 60695-11-10
Flash Point 480 °C896 °Fignition; ASTM D1929
 550 °C1020 °Fself ignition; ASTM D1929
Oxygen Index 28 %28 %Method A; ISO 4589-1/-2
Glow Wire Ignition Temperature  875 °C
@Thickness 0.750 mm
1610 °F
@Thickness 0.0295 in
IEC 60695-2-13
 875 °C
@Thickness 1.50 mm
1610 °F
@Thickness 0.0591 in
IEC 60695-2-13
 900 °C
@Thickness 3.00 mm
1650 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  850 °C
@Thickness 1.00 mm
1560 °F
@Thickness 0.0394 in
IEC 60695-2-12
 875 °C
@Thickness 1.50 mm
1610 °F
@Thickness 0.0591 in
IEC 60695-2-12
 930 °C
@Thickness 3.00 mm
1710 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5841.584ISO 489
Haze <= 0.50 %
@Thickness 3.00 mm
<= 0.50 %
@Thickness 0.118 in
ISO 14782
Transmission, Visible  <= 89 %
@Thickness 3.00 mm
<= 89 %
@Thickness 0.118 in
ISO 13468-2
 <= 89 %
@Thickness 4.00 mm
<= 89 %
@Thickness 0.157 in
ISO 13468-2
 90 %
@Thickness 1.00 mm
90 %
@Thickness 0.0394 in
ISO 13468-2
 90 %
@Thickness 2.00 mm
90 %
@Thickness 0.0787 in
ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection Molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 India
 Near East/Africa
 North America
 South and Central America
Eff. thermal diffusivity (m²/s)1E-07
FeatureRelease agent
FormPellets
ProcessInjection Molding
UL recognitionUL\l1.5\n
 UL\lh\n

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® LED2643 Polycarbonate
Covestro Makrolon® AL 2647 Polycarbonate, Automotive Lens Injection Grade
Röhm Plexiglas® 8N PMMA Molding Compound
Covestro Makroblend® UT5205 PC/PBT Blend
Covestro Makrolon® LED2045 Polycarbonate

PB09959 / 92799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.