MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ CC174-N PTFE, 15% Fiberglass/Moly Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Product Form: Gray, non-pelletized powder. Applications include bearings, rider rings, and packings.

Data provided by Dyneon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.520 g/cc0.0188 lb/in³ASTM D4894
Density 2.27 g/cc0.0820 lb/in³ASTM D792
Particle Size 25 µm25 µmASTM D4894
Deformation 3.0 %
@Pressure 15.00 MPa
3.0 %
@Pressure 2175 psi
ASTM D621
 5.0 %
@Time 86400 sec,
Pressure 15.00 MPa
5.0 %
@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060value after 15 sec; ASTM D2240
 6767initial value; ASTM D2240
Tensile Strength at Break 23.4 MPa3390 psiASTM D4894
Elongation at Break 240 %240 %ASTM D4894
Tensile Modulus 0.152 GPa22.0 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
CTE, linear  101 µm/m-°C
@Temperature 30.0 - 100 °C
56.0 µin/in-°F
@Temperature 86.0 - 212 °F
ASTM E831
 137 µm/m-°C
@Temperature 100 - 200 °C
76.0 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
 171 µm/m-°C
@Temperature 200 - 300 °C
95.0 µin/in-°F
@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity  0.270 W/m-K
@Temperature 250 °C
1.87 BTU-in/hr-ft²-°F
@Temperature 482 °F
ASTM E1530
 0.280 W/m-K
@Temperature 100 °C
1.94 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1530
Shrinkage 1.9 %1.9 %ASTM D4894

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC FC 472 PTFE, 5% Glass/ 5% Moly
AGC FC 411 PTFE, 5% Moly
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Beijing Evergrow Resources PTFE, 15% Glass Fiber, 10% Polyimide, 5% Graphite Filled
AGC FC 482 PTFE, 55% Bronze/ 5% Moly

PDYM62 / 34674

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.