MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell SEQUEL® 1780 Engineered Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Description: SEQUEL® 1780 engineered polyolefin is designed for mold-in-color or partially painted automotive exterior applications that require dimensional stability over a broad temperature range with enhanced scratch and mar resistance. This material exhibits excellent processability and low-temperature properties.

Applications: Bumper side claddings, rockers, and other components that demand close dimensional tolerances

Information provided by Solvay Engineered Polymers.

LyondellBasell acquired Solvay Engineered Polymers in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/inas molded; ISO 294
Melt Flow 21 g/10 min21 g/10 minCondition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psi50 mm/min; ASTM D638
Flexural Modulus 1.38 GPa200 ksiI.B., TAN, 0.5 in/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
28.9 µin/in-°F
@Temperature -22.0 - 176 °F
ASTM E228

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zylog Hipolyene® 1048 X1 Thermoplastic Polyolefin & PP Compound
Solvay Engineered Polymers SEQUEL® 1440LS TPO
Phillips Sumika Marlex® CHN-200 Thermoplastic Polyolefin
Omni Plastics OmniPro™ TPO MF20 HF HSV Thermoplastic Polyolefin
Omni Plastics OmniPro™ TPO 20M HC Thermoplastic Polyolefin

PSOLE12 / 68018

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.