MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Ametek Tungsten-Copper Composites AWC 9010
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Information supplied by Ametek Specialty Metal Products.

The material is available as finished parts with the following maximum dimensions:

Width: 6 inches (152 mm)
Thickness: 0.150 inches (3.8 mm)
Length: 8 inches (203 mm)

These composites of tungsten and copper have many applications in electronic devices. The excellent thermal conductivity and low thermal expansion makes them ideal for: chip mounting, heat sinks, circuit board cores, lids or covers, or thermal spreaders. The material can be machined into shapes and readily plated if required. AMETEK's wrought powder metallurgy composites have superior through-thickness thermal conductivity versus other products.

Key Words: Tungsten Alloy
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 16.98 g/cc0.6134 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear  6.51 µm/m-°C
@Temperature 30.0 - 150 °C
3.62 µin/in-°F
@Temperature 86.0 - 302 °F
 6.53 µm/m-°C
@Temperature 30.0 - 800 °C
3.63 µin/in-°F
@Temperature 86.0 - 1470 °F
 6.70 µm/m-°C
@Temperature 30.0 - 400 °C
3.72 µin/in-°F
@Temperature 86.0 - 752 °F
Thermal Conductivity 175 W/m-K1210 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 10 %10 %
Tungsten, W 90 %90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Applied Composites 120 Polyester SMC
Applied Composites 150 Polyester SMC
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
Ametek Tungsten-Copper Composites AWC 8515
Ametek Tungsten-Copper Composites AWC 8020

NMA274 / 18193

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.