MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer

Material Notes: Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistance, and ease of cleaning expected of PVF film. Tedlar® SP also offers custom color capability not previously available in PVF film. Tedlar® SP is an unoriented film. It possesses high elongation and moderate yield stress. After lamination using conventional means, it can be easily embossed and will maintain high pattern definition. Tedlar® SP can also be subjected to high levels of forming without significant recovery stresses.

Key Words: PVF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption at Equilibrium 0.50 %0.50 %ASTM D570
Moisture Vapor Transmission 0.750 cc-mm/m²-24hr-atm1.90 cc-mil/100 in²-24hr-atmASTM E96E-80
Thickness 25.4 microns1.00 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 41.0 MPa5950 psiASTM D882-80, Method A - 100%
Elongation at Break 200 %200 %ASTM D882-80
Coefficient of Friction 0.210.21Film:Metal; ASTM D1894
Tear Strength 550 kN/m3140 pliGraves, MD; ASTM D1004
 550 kN/m3140 pliGraves, TD; ASTM D1004
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+13 ohm-cm4.00e+13 ohm-cmASTM D257-78
Dielectric Constant 7.07.0ASTM D151-81
Dielectric Strength 118 kV/mm3000 kV/inASTM D151-81
Dissipation Factor 0.00200.0020ASTM D151-81
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FMD and TD; ASTM D696-79
Specific Heat Capacity 1.01 J/g-°C0.241 BTU/lb-°FDuPont 990 test
Maximum Service Temperature, Air 107 °C225 °FContinuous
 175 °C347 °FShort Cycle
Minimum Service Temperature, Air -72.0 °C-97.6 °FContinuous
Shrinkage <= 2.0 %
@Temperature 170 °C
<= 2.0 %
@Temperature 338 °F
ASTM D1204-78
 0.80 %
@Temperature 50.0 °C,
Time 1800 sec
0.80 %
@Temperature 122 °F,
Time 0.500 hour
 1.5 %
@Temperature 100 °C,
Time 1800 sec
1.5 %
@Temperature 212 °F,
Time 0.500 hour
 1.8 %
@Temperature 150 °C,
Time 1800 sec
1.8 %
@Temperature 302 °F,
Time 0.500 hour
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.461.46ASTM D542-50
Haze 0.60 %0.60 %Internal; Gardner
 2.6 %2.6 %Total; Gardner
Gloss 57 %57 %20°; Gardner
 81 %81 %60°; Gardner
 93 %93 %85°; Gardner
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature 105 - 171 °C221 - 340 °FFilm Forming Surface Temperature
 
Descriptive Properties
Resistance to AcidsNo Visible Effect2 hr Boiling
Resistance to BasesNo Visible EffectImmersion
WeatherabilityExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TTR10SH9 Clear Polyvinyl Fluoride Film
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film

PDU9301 / 138474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.