MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® 909 BK Flame Retardant Nylon 66/6, 25% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Vydyne 909 is an halogenated, 25% glass filled, flame retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4mm (0.016") thick.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ISO 1183
Water Absorption 0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.3 %1.3 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
0.0040 in/in
@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
0.010 in/in
@Thickness 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psiConditioned; ISO 527-2
 132 MPa19100 psiDry; ISO 527-2
Elongation at Break 2.2 %2.2 %Dry; ISO 527-2
 3.0 %3.0 %Conditioned; ISO 527-2
Tensile Modulus 7.10 GPa1030 ksiConditioned; ISO 527-2
 9.10 GPa1320 ksiDry; ISO 527-2
Flexural Strength 140 MPa20300 psiConditioned; ISO 178
 193 MPa28000 psiDry; ISO 178
Flexural Modulus 5.00 GPa725 ksiConditioned; ISO 178
 8.30 GPa1200 ksiDry; ISO 178
Poissons Ratio 0.400.40Dry; ISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 180
Charpy Impact Unnotched  3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.940 J/cm²
@Temperature 23.0 °C
4.47 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.950 J/cm²
@Temperature -30.0 °C
4.52 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
60 - 120 sec
@Thickness 0.118 in
PLC 6; ASTM D495
Comparative Tracking Index 250 - 399 V
@Thickness 3.00 mm
250 - 399 V
@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI  >= 120 sec
@Thickness 0.750 mm
>= 120 sec
@Thickness 0.0295 in
PLC 0; UL 746
 >= 120 sec
@Thickness 1.50 mm
>= 120 sec
@Thickness 0.0591 in
PLC 0; UL 746
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
PLC 0; UL 746
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
PLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minPLC 3; UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
11.1 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 250 °C482 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FISO 75-2/A
UL RTI, Electrical 65.0 °C149 °FUL 746
 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.400 mm
149 °F
@Thickness 0.0157 in
UL 746
 65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 95.0 °C
@Thickness 1.50 mm
203 °F
@Thickness 0.0591 in
UL 746
 95.0 °C
@Thickness 3.00 mm
203 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 0.400 mm
149 °F
@Thickness 0.0157 in
UL 746
 110 °C
@Thickness 0.750 mm
230 °F
@Thickness 0.0295 in
UL 746
 110 °C
@Thickness 1.50 mm
230 °F
@Thickness 0.0591 in
UL 746
 110 °C
@Thickness 3.00 mm
230 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
Oxygen Index 32 %32 %ISO 4589-1/-2
Glow Wire Ignition Temperature  750 °C
@Thickness 0.750 mm
1380 °F
@Thickness 0.0295 in
IEC 60695-2-13
 750 °C
@Thickness 1.50 mm
1380 °F
@Thickness 0.0591 in
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
IEC 60695-2-13
 930 °C
@Thickness 0.400 mm
1710 °F
@Thickness 0.0157 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 270 °C464 - 518 °FInjection Molding
Middle Barrel Temperature 240 - 270 °C464 - 518 °FInjection Molding
Front Barrel Temperature 240 - 270 °C464 - 518 °FInjection Molding
Nozzle Temperature 240 - 270 °C464 - 518 °FInjection Molding
Melt Temperature 250 - 270 °C482 - 518 °FInjection Molding
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection Molding
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Injection Molding
 
Descriptive Properties
Automotive SpecificationsDelphi M6538V
 GM GMP.PA66.058
FeaturesFlame Retardant
 Good Crack Resistance
 Good Mold Release
 Good Toughness
 Halogenated
 High Rigidity
 High Strength
 Ignition Resistant
 Lubricated
Suggested Max Regrind (%)25
UsesAppliances
 Automotive Electronics
 Bobbins
 Circuit Boards, Printed
 Connectors
 Electrical Parts
 Electrical/Electronic Applications
 Fasteners
 Hinges, Living
 Housing, Electrical
 Industrial Applications
 Lighting Applications
 Switches

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TW200F6 PA46-GF30, Conditioned, 30% Glass Filled, Heat Stabilized
Envalior Stanyl® TW241F12 PA46-GF60, Conditioned, 60% Glass Filled, Heat Stabilized
BASF Ultramid® A3WG6 30% Glass Filled PA66 (Dry)
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry)
Delrin Delrin® 500P BK602 POM

PZASCE9721 / 220824

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.