MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for machined parts in food processing equipment. HYDEX® 4101 has excellent resistance to typical cleaning chemicals such as chlorine and caustic solutions and has a very low moisture absorption rate, as much as 15 times less than nylon.

  • Good chemical resistance properties
  • High impact strength
  • FDA approved for use in food processing
  • A wear factor up to 50% better than PET-P
  • Very low moisture absorption rate
  • Excellent machining qualities
  • No center line porosity

HYDEX® 4101 & 4101L exhibits a broad range of outstanding properties for a variety of applications, especially in the food processing industry. It is ideal for applications such as cams, bearings, gears, food pistons, wear strips, scraper blades, valve bodies and conveyor components.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D792
Water Absorption 0.070 %
@Time 86400 sec
0.070 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 49.6 MPa7200 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Tensile Modulus 2.62 GPa380 ksiASTM D638
Flexural Modulus 2.69 GPa
@Temperature 22.8 °C
390 ksi
@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.110.11vs Steel; LNP EPALP-TB001
Coefficient of Friction, Static 0.0800.080Steel; LNP EPALP-TB001
K Factor (Wear Factor) 3838in5-min/ft-lbs/hr, at 2000 PV; LNP EPALP-TB001
Limiting Pressure Velocity 0.550 MPa-m/sec15700 psi-ft/minLNP EPALP-TB003, at 100 ft/min
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FUL746B
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C195 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYes
FDA YesYes
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger HYDEX® 4101 Polybutylene Terephthalate (PBT)
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
Mitsubishi Chemical Advanced Materials Ertalyte™ TX Internally Lubricated Semi-Crystalline PET
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)

PENSIN037 / 92854

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.