MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 5000 Dimethylpolysiloxane Polymer
Categories: Polymer

Material Notes: BLUESIL FLD 47 V 5 000 to 47 V 1 000 000 (viscosities 5 000 - 10 000 - 12 500 - 30 000 - 60 000 - 300 000 – 500 000 - 1 000 000) are dimethylpolysiloxane polymers with linear chains.

Applications: BLUESIL FLD 47 V 5 000 to 47 V 1 000 000 can be used as:

  • Antiadherent agents: mould release of plastics and metal castings,
  • Lubricants: lubrication of elastomers and plastics on metal,
  • Hydraulic damping fluids,
  • Additives in maintenance products (wax polishes, floor and furniture polishes...).
Advantages:
  • Excellent thermal stability.
  • Good resistance to combustion.
  • Good dielectric properties.
  • Low freezing point.
  • Low surface tension.
  • High compressibility.
  • Good oxidation resistance.
  • Absence of ageing under exposure to weather conditions.
  • Low variation of viscosity with temperature.
  • Good shear resistance.
  • Non miscible with most of organic materials.
  • Soluble in aromatic, aliphatic and chlorinated solvents.
  • Insoluble in water and alcohols.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.973 g/cc0.973 g/cc
Kinematic Viscosity 5000 cSt5000 cSt
Surface Tension 21.1 dynes/cm21.1 dynes/cm
Storage Temperature -20.0 - 50.0 °C-4.00 - 122 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Dielectric Constant 2.82.8
Dielectric Strength 18.0 kV/mm457 kV/in
Dissipation Factor 0.000110.00011
 
Thermal PropertiesMetricEnglishComments
CTE, linear 94.5 µm/m-°C
@Temperature 20.0 - 100 °C
52.5 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 1.50 J/g-°C
@Temperature 40.0 - 200 °C
0.359 BTU/lb-°F
@Temperature 104 - 392 °F
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°F
Pour Point -45.0 °C-49.0 °F
Flash Point >= 300 °C>= 572 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4041.404
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Appearanceclear - colorless liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 1000000 Dimethylpolysiloxane Polymer
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 50 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FB Silicone Gum
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 10000 Dimethylpolysiloxane Polymer
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 20 Polydimethylsiloxanic Fluids

PBLUST108 / 191084

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.