MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema OREVAC® 18910 Maleic Anhydride Modified Copolymer
Categories: Polymer; Adhesive; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene; SMA Polymer

Material Notes: OREVAC® 18910 is anhydride modified copolymer based on styrenic and ethylenic copolymers. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefin resins. OREVAC® 18910 is typically used as adhesive to bond PS, PE, EVOH and PA in coextruded multilayer structures like films or sheets.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc
@Temperature 23.0 °C
0.0343 lb/in³
@Temperature 73.4 °F
ISO 1183
Melt Index of Compound 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 117 °C243 °FDSC
Vicat Softening Point 77.0 °C171 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema OREVAC® 18350 Grafted Maleic Anhydride Polyethylene
Arkema OREVAC® 18365 Maleic Anhydride Modified Polyethylene
Arkema OREVAC® 18360 Maleic Anhydride Modified Polyethylene
Arkema OREVAC® 18510 Grafted Maleic Anhydride Polyethylene
Dow Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate

PARKG149 / 80103

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.