MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubriplate PURE TAC PURE Aluminum Complex USP Mineral Oil-Based Food Machinery Grade Grease
Categories: Fluid; Lubricant; Aluminum Gellant

Material Notes: This tacky, adhesive, highly water resistant, Class H-1 grease is designed for applications subjected to chemically treated water, heat and steam. For all types of medium to slow speed bearings, open gears and hydrostatic cooker chains.

PURE TAC is available in Cartridges, Pails, 1/4 Drums and Drums.

H-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.

Information provided by Lubriplate

Key Words: Part Number L0236-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Saybolt Viscosity at 100°F 6500 SUS6500 SUS
Kinematic Viscosity at 40°C (104°F) 1187 cSt1187 cSt
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 265265Unknown Amount of Work
Penetration P(60), 1/10 mm 295295Unknown Amount of Work
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -3.89 °C25.0 °FApprox. Cold test
Dropping Point 271 °C520 °FASTM Test
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Antiwear (AW)/ Extreme Pressure (EP)AW
NLGI Grade2
Rust/Oxidative AdditivesYES
Water ResistantYES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum, Al
Indium Corp. Indalloy 192 Pure Aluminum
Alclad Aluminum 2014-T4, T451
Aluminum 5052-H32
Aluminum 2014-T4; 2014-T451

WLUBR182 / 76228

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.