MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYBATCH™ ASP-2000 Permanent Antistatic Product
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Description

POLYBATCH® ASP-2000 is a permanent antistatic product. This material is designed to provide immediate antistatic performance and last throughout the lifetime of the polyolefin. POLYBATCH® ASP-2000 will not bloom to the surface and will therefore not interfere with printing. POLYBATCH® ASP-2000 performance is maximized when processed at temperatures between 190 to 230°C (375 to 446°F).
Application

POLYBATCH® ASP-2000 is typically recommended for us in blown film, injection molding, and blow molding applications at 10 to 15% addition levels depending upon application requirements. This product is not recommended for use in cast film applications.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBLAK™ 4651SF Universal Black Color Concentrate, 50% Carbon Black in EVA
A. Schulman POLYBATCH™ AF-1085 Antifog Concentrate
A. Schulman POLYBATCH™ ASC-331 Inorganic Antislip Masterbatch Based in Polyethylene
A. Schulman POLYBATCH™ FSU-105 Concentrate Based In LDPE
A. Schulman POLYBATCH™ U-0294-L Blowing Agent Concentrate Based In PE

PASHU370 / 25334

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.