MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

A. Schulman Diamond ASA S510
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact

Information provided by Diamond Polymers, Inc.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow  1.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
 3.7 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.7 g/10 min
@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ASTM D785
Tensile Strength, Yield 44.1 MPa6400 psichs 2 in/min; ASTM D638
Flexural Modulus 2.28 GPa330 ksiTangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched 2.08 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
3.90 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C181 °F0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point 92.2 °C198 °F0.125 inch, 1 Kg; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 229 - 260 °C445 - 500 °F
Middle Barrel Temperature 232 - 266 °C450 - 510 °F
Front Barrel Temperature 235 - 271 °C455 - 520 °F
Nozzle Temperature 221 - 271 °C430 - 520 °F
Melt Temperature 221 - 271 °C430 - 520 °FMelt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Mold Temperature 37.8 - 82.2 °C100 - 180 °FHigher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products.
Drying Temperature 80.0 - 85.0 °C176 - 185 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.10 %<= 0.10 %
Back Pressure 0.517 - 1.03 MPa75.0 - 150 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond ASA S150
A. Schulman Diamond ASA S210B
EMS-Grivory Grilamid® L 25 W 40 PA12
EMS-Grivory Grilamid® LV-3H PA12-GF30
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, Dry as Molded

PDIAM248 / 30086

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.