MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1899 X 141360 Z Acrylic (PMMA); FDA Compliant Ingredients - Permanently Static Dissipative - ESD Protection - UV Stabilized - Transparent Grade
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: This compound has been formulated to meet the static dissipative requirements of the ATEX Directive.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 33.1 MPa4800 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.31 GPa190 ksiASTM D 638
Flexural Strength 48.3 MPa7000 psiASTM D 790
Flexural Modulus 1.38 GPa200 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 6.41 J/cm
@Thickness 3.20 mm
12.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+9 ohm<= 1.00e+9 ohmESD STM11.11
Static Decay <= 2.0 sec<= 2.0 secFTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 218 °C360 - 425 °F
Mold Temperature 79.4 - 107 °C175 - 225 °F
Drying Temperature 93.3 °C
@Time 14400 sec
200 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 2560.6 Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company PermaStat® 101 Polypropylene (PP); Glass Fiber - Permanently Anti-static - ESD Protection
RTP Company RTP 1800 A Z Polycarbonate/Acrylic Alloy (PC/PMMA), FDA Compliant Ingredients
RTP Company RTP 1899 X 136863 J Acrylic (PMMA); ESD Protection - Permanently Static Dissipative - Transparent
RTP Company RTP 2099 X 134682 Polycarbonate/PBT Alloy; Permanently Static Dissipative - ESD Protection - Impact Modified - UV Stabilized

PQZRA32360 / 205828

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.