MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical HF380 ABS, Injection Molding
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: High Flow

Applications: Electric/Electronic Products, Miscellaneous Goods

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 42 g/10 min
@Load 10.0 kg,
Temperature 220 °C
42 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D785
Tensile Strength, Yield 44.0 MPa
@Thickness 3.20 mm
6390 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break >= 10 %
@Thickness 3.20 mm
>= 10 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield 5.0 %
@Thickness 3.20 mm
5.0 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Tensile Modulus 2.05 GPa
@Thickness 3.20 mm
297 ksi
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Strength 71.0 MPa
@Thickness 3.20 mm
10300 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.35 GPa
@Thickness 3.20 mm
341 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  1.20 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
2.24 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 1.20 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
2.24 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 2.45 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
4.59 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 2.45 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
4.59 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
@Thickness 6.40 mm
185 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 93.0 °C
@Load 5.10 kg
199 °F
@Load 11.2 lb
50°C/h; ASTM D1525
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 200 °C356 - 392 °F
Middle Barrel Temperature 190 - 210 °C374 - 410 °F
Front Barrel Temperature 200 - 220 °C392 - 428 °F
Nozzle Temperature 200 - 230 °C392 - 446 °F
Melt Temperature 210 - 240 °C410 - 464 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F
Drying Temperature 70.0 - 80.0 °C
@Time 7200 - 14400 sec
158 - 176 °F
@Time 2.00 - 4.00 hour
Moisture Content >= 0.010 %>= 0.010 %
Back Pressure 0.490 - 1.47 MPa71.1 - 213 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical SG175 ABS, Super Surface Gloss
LG Chemical HI855M PMMA, Impact Resistant Grade
LG Chemical AF342 ABS, Flame Retardant
AISI 1213 Steel, hot rolled, 19-38 mm round
LG Chemical AF312 ABS, Flame Retardant

PLHCHEM9939 / 239455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.