MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alpha-2 Titanium Aluminide, Ti3Al
Categories: Metal; Intermetallic

Material Notes: Intermetallic aluminides have good mechanical properties and stability to be used in high temperature environments. A thin protective Al2O3 coating forms to provide oxidative stability. A range of stoichiometries is possible through elemental substitutions. Researchers are examining titanium aluminide applications in fields such as jet engine turbines because of their high temperature properties and low density.

May be cast. Difficult to process by ingot metallurgy, forging, or sheet rolling.

Key Words: Ti3Al
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.20 g/cc0.152 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 800 - 1140 MPa116000 - 165000 psi
Tensile Strength, Yield 700 - 990 MPa102000 - 144000 psi
Elongation at Break 0.00 - 10 %0.00 - 10 %
Modulus of Elasticity 145 GPa21000 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 1600 °C2910 °F
Maximum Service Temperature, Air 650 °C1200 °FOxidation Limit
Maximum Service Temperature, Inert 760 °C1400 °FCreep Limit
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 15.8 %15.8 %by weight
Titanium, Ti 84.2 %84.2 %by weight
 
Descriptive Properties
Critical Ordering Temperature1100°C
Crystal StructureD019Ordered HCP

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gamma Titanium Aluminide, TiAl
Titanium Aluminide, TiAl3
Ti-24Al-11Nb Titanium Aluminide
Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 850°C (1560°F) + Aged 510°C 8 hr
Titanium, Ti

MIAL000 / 12198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.